Polymer Property : Compressive Yield Strength = 68700 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 474 MPa

@Temperature 232 °C
68700 psi

@Temperature 450 °F
Phase V (Prepreg stored in freezer 1 year at -9°C and exposed to 60 days at RT)
Hexcel® HexPly® F650 Bismaleimide Resin with Graphite F3T584 fabric reinforcement
Aging Data, (T300-3K, 8 H.S.); Laminate Physicals: 59.6% Fiber volume, 34.0% Resin content, 1.0% VoidsInformation provided by HexCel
Compressive Yield Strength 474 MPa

@Temperature 24.0 °C
68700 psi

@Temperature 75.2 °F
Hexcel® HexPly® F263 Epoxy Resin, 120 Glass Fabric
Hexcel designation: 120-38"-F263; Fiber: 450-1/2Information provided by HexCel