Polymer Property : Compressive Yield Strength = 5.08 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 0.0350 MPa

@Strain 25.0 %
5.08 psi

@Strain 25.0 %
BS ISO 7214 1998
Zotefoams Plastazote® MP15FR Metallocene Polyethylene Foam, Flame Retardant
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Compressive Yield Strength 0.0350 MPa

@Strain 25.0 %
5.08 psi

@Strain 25.0 %
ASTM 1056/85
Eurofoam Porocell POR 304 CM-RS EPDM Foam
Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l.
Compressive Yield Strength 0.0350 MPa

@Strain 25.0 %
5.08 psi

@Strain 25.0 %
ASTM 1056/85
Eurofoam Porocell POR 300/60 Ethylene Octane Metallocene EPDM Foam
Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l.
Compressive Yield Strength 0.0350 MPa

@Strain 25.0 %
5.08 psi

@Strain 25.0 %
ASTM 1056/85
Eurofoam Porocell POR 304 CM EPDM Foam
Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l.
Compressive Yield Strength 0.0350 MPa

@Strain 25.0 %
5.08 psi

@Strain 25.0 %
ASTM 1056/85
Eurofoam Porocell POR 304 CM-BI EPDM Foam
Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l.
Compressive Yield Strength 0.0350 MPa

@Strain 25.0 %
5.08 psi

@Strain 25.0 %
ASTM 1056/85
Eurofoam Porocell POR 304 CM-GR EPDM Foam
Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l.