Mechanical Properties Metric English Comments
Compressive Yield Strength 5.00 MPa

@Strain 1.00 %
725 psi

@Strain 1.00 %
ISO 604
Murtfeldt Original Material ”S”® Black Antistatic Polyethylene, Conductive
Original Material ”S”® black has the same properties as Original Material ”S”® green/natural. In addition, it is also electrostatically conductive due to the addition of additives. Special Pro..