Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 478 MPa @Temperature 23.0 °C |
69300 psi @Temperature 73.4 °F |
|
Hexcel® HexPly® F652 Bismaleimide Resin, Carbon Fabric Form Material Description: F3G584-60; Fiber: T300-3K; T300/13.5 mils (0.343 mm) per plyInformation provided by HexCel |