Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 324 MPa @Temperature 25.0 °C |
47000 psi @Temperature 77.0 °F |
After 2000 in-inlb/in impact |
Hexcel® HexPly® 8551-7 Epoxy Matrix, IM7 Fiber Information provided by HexCel |
|||
Compressive Yield Strength | 324 MPa @Temperature 232 °C |
47000 psi @Temperature 450 °F |
Press Cured; Tested at 232°C after 500 hours at 232°C |
Hexcel® HexPly® F652 Bismaleimide Resin, Carbon Fabric Form Material Description: F3G584-60; Fiber: T300-3K; T300/13.5 mils (0.343 mm) per plyInformation provided by HexCel |