Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 282 MPa @Temperature 23.0 °C |
40900 psi @Temperature 73.4 °F |
Compression After Impact @ 6.7 J/mm; AITM 1.0010 |
Hexcel® HexPly® M48 180°C/356°F Curing Epoxy Matrix, M48/35%/150/IM7 GS Fiber: IM7 GS, UD, 150 g/m2Information provided by HexCel |
|||
Compressive Yield Strength | 282 MPa @Temperature 23.0 °C |
40900 psi @Temperature 73.4 °F |
Compression After Impact @ 6.7 J/mm; AITM 1.0010 |
Hexcel® HexPly® M48 180°C/356°F Curing Epoxy Matrix, M48/42%/G1094/1000 Fiber: T800H 6K, 5H Satin weave, 290 g/m2Information provided by HexCel |