Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 365 MPa @Temperature 204 °C |
52900 psi @Temperature 399 °F |
0° |
Hexcel® HexPly® 954-2A Curing Cyanate Resin, S-2 Glass Fiber Reinforced 8 Harness Satin Fabric Information provided by HexCel |