Mechanical Properties Metric English Comments
Compressive Yield Strength 248 MPa

@Temperature 104 °C
36000 psi

@Temperature 219 °F
Open hole compression, Wet
Hexcel® HexPly® 8551-7 Epoxy Matrix, IM7 Fiber
Information provided by HexCel