Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 236 MPa @Temperature 25.0 °C |
34200 psi @Temperature 77.0 °F |
0°, Wet, Fill Compression |
Hexcel® HexPly® 8552 Epoxy Matrix, IM7 Fiber Information provided by HexCel |
|||
Compressive Yield Strength | 236 MPa @Temperature 149 °C |
34200 psi @Temperature 300 °F |
Open Hole Compression; Wet |
Hexcel® HexPly® 954-2A Curing Cyanate Resin, IM7 Fiber Information provided by HexCel |