Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 234 MPa @Temperature 25.0 °C |
34000 psi @Temperature 77.0 °F |
After 1500 in-in-lb/in impact, Dry |
Hexcel® HexPly® 8552 Epoxy Matrix, IM7 Fiber Information provided by HexCel |