Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 22.8 MPa @Strain 1.00 % |
3300 psi @Strain 1.00 % |
ASTM D695 |
Saint-Gobain Meldin® 7022 DF Direct Formed Graphite Filled Polyimide Melidin® 7022 DF is a direct formed polyimide that contains 40% graphite filler. This grade offers additional dimensional stability at elevated temperatures and the lowest CTE of any Meldin® .. |