Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 1321 MPa @Temperature 23.0 °C |
191600 psi @Temperature 73.4 °F |
prEN2580 Type B |
Hexcel® HexPly® M48 180°C/356°F Curing Epoxy Matrix, M48/35%/150/AS7 GS Fiber: AS7 GS, UD, 150 g/m2Information provided by HexCel |