Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 175.1 MPa @Temperature 232 °C |
25400 psi @Temperature 450 °F |
Wet condition - 96 hours in boiling H2O |
Hexcel® HexPly® F650 Bismaleimide Resin with Fiberglass 7781 fabric reinforcement Laminate Physicals: 53% Fiber volume, 29% Resin content, 0.5% VoidsInformation provided by HexCel |