Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 9.50 MPa

@Strain 1.00 %
1380 psi

@Strain 1.00 %
ISO 604
Murtfeldt Original Material ”S”® plus + GB Polyethylene, Glass Bead Filled
The balanced quantity of micro glass beads in Material ”S”® plus+ GB provides the combined benefits of extremely high molecular weight polyethylene and glass. The glass beads that protrude from ..