Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 128 MPa @Strain 10.0 % |
18500 psi @Strain 10.0 % |
ASTM D695 |
Saint-Gobain Meldin® 7001 CM Compression Molded Polyimide Meldin® 7001 CM unfilled polyimide base resin, compression moldedSpecification Qualifications:Satisfies Type I P for ASTM D 6456-99: Standard Specification for Finished Parts Made from Polyimide .. |
|||
Compressive Yield Strength | 128 MPa @Temperature 24.0 °C |
18600 psi @Temperature 75.2 °F |
Wet |
Hexcel® F161 Epoxy Resin, 285 Kevlar Fabric Hexcel designation: 285-38"-F161; Fiber: Kev. 49 1140Information provided by HexCel |