Polymer Property : Compressive Yield Strength = 12.0 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 0.0345 - 0.0827 MPa

@Strain 25.0 %
5.00 - 12.0 psi

@Strain 25.0 %
Range, 0.2"/min. strain rate
Rogers Corporation Poron® 4701-30-25 Urethane Foam, Very Soft
Very soft, easily compressed for use where flexibility is a key requirement.  Standard available  thickness range from 0.021"Features and Benefits of PORON Products: Excellent compression set resi..
Compressive Yield Strength 0.0345 - 0.0827 MPa

@Strain 25.0 %
5.00 - 12.0 psi

@Strain 25.0 %
Range, 0.2"/min. strain rate
Rogers Corporation Poron® 4701-30-25037 P Urethane Foam, Very Soft, Supported with Clear Polyester Film
Very soft, easily compressed for use where flexibility is a key requirement.  Standard available  thickness range from 0.021"Features and Benefits of PORON Products: Excellent compression set resi..
Compressive Yield Strength 0.0345 - 0.0827 MPa

@Strain 25.0 %
5.00 - 12.0 psi

@Strain 25.0 %
Range, 0.2"/min. strain rate
Rogers Corporation Poron® 4701-30-25047 P Urethane Foam, Very Soft, Supported with Clear Polyester Film
Very soft, easily compressed for use where flexibility is a key requirement.  Standard available  thickness range from 0.021"Features and Benefits of PORON Products: Excellent compression set resi..
Compressive Yield Strength 0.0345 - 0.0827 MPa

@Strain 25.0 %
5.00 - 12.0 psi

@Strain 25.0 %
Range, 0.2"/min. strain rate
Rogers Corporation Poron® 4701-30-25 Supported Urethane Foam, Very Soft, Supported with Clear Polyester Film
Very soft, easily compressed for use where flexibility is a key requirement. Contains PET film reinforcement.Features and Benefits of PORON Products: Excellent compression set resistance which enab..