Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 0.103 - 0.310 MPa @Strain 25.0 % |
15.0 - 45.0 psi @Strain 25.0 % |
Range, 0.2"/min. strain rate |
Rogers Corporation Poron® 4701-50 Supported Urethane Foam, Firm, PET Supported Firm material used for managing high energy impact with gasketing needs. Standard available thickness range from 0.012" to 0.500" (0.30 mm to 12.7 mm).Features and Benefits of PORON Products: Exce.. |
|||
Compressive Yield Strength | 0.0345 - 0.310 MPa @Strain 25.0 % |
5.00 - 45.0 psi @Strain 25.0 % |
Range, 0.2"/min. strain rate |
Rogers Corporation Poron® 4701-50 Thin as Cast Urethane Foam, Firm, Thin as Cast Firm material used for managing high energy impact with gasketing needs. Standard available thickness range from 0.012" to 0.500" (0.30 mm to 12.7 mm).Features and Benefits of PORON Products: Exce.. |