Polymer Property : Ball Indentation Hardness = 8120 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Ball Indentation Hardness 56.0 MPa
8120 psi
DIN 53456
Global PP-2500-PC Polypropylene Block Copolymer
Description-opacity, medium to high stiffness, high impact strength at low temperatureApplications-thin walled containers, tool boxes, food containersInformation provided by Global Polymers Corporat..
Ball Indentation Hardness 56.0 - 60.0 MPa
8120 - 8700 psi
ISO 2032-N132
Adamas Adalon® 433 PTFE, 10% Ekonol®
Information provided by Adamas, HPM