Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 58.0 - 64.0 MPa | 8410 - 9280 psi | ISO 2032-N132 |
Adamas Adalon® 401 PTFE, 10% Polyimide Information provided by Adamas, HPM |
|||
Ball Indentation Hardness | 60.0 - 64.0 MPa | 8700 - 9280 psi | ISO 2032-N132 |
Adamas Adalon® 992 Modified PTFE Information provided by Adamas, HPM |