Polymer Property : Ball Indentation Hardness = 61.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Ball Indentation Hardness 61.0 MPa
8850 psi
DIN 53456
Global PP-3200-H Polypropylene Random Copolymer
Description-medium stiffness, low melting temperatures, very good for seal Applications-sheets, bottlesInformation provided by Global Polymers Corporation.
Ball Indentation Hardness 61.0 MPa
8850 psi
H 358/30; ISO 2039
Borealis Daplen™ EF267AI Polypropylene TPO Compound
Daplen™ EF267AI is a 20 % mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process...