Ball Indentation Hardness 400 MPa
58000 psi
ISO2039.1 DIN.53456
Omnia Plastica PPS GF40 Polyphenylenesulphide
Crystalline polymer based on polyphenylene sulfide with the addition of 40% glass-fibre. Very high rigidity, stiffness and flexural strength. The temperature resistance is very high: up to 240° C. ..
Ball Indentation Hardness 400 MPa
58000 psi
H 961/30; ISO 2039/P1
Hexion Bakelite™ EP 8412 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage
Epoxy molding compound, inorganically filled, glass fiber reinforced, heat resistant, dimensionally stable, good electrical and mechanical properties, very good chemical resistance, low viscosity, U..
Ball Indentation Hardness 400 MPa
58000 psi
H 961/30; ISO 2039/P1
Hexion Bakelite™ PF 2874 Phenolic Formaldehyde Resin, Low Shrinkage, Improved Electrical Properties, UL Listed, High Mechanical Strength
Phenolic molding compound, inorganically filled, glass fiber reinforced, increased mechanical strength, increased temperature stability, low water absorption, good dimensional stability, UL listed m..
Ball Indentation Hardness 400 MPa
58000 psi
H 961/30; ISO 2039/P1
Hexion Bakelite™ PF 6501 Phenolic Formaldehyde Resin, Low Shrinkage
Phenolic molding compound, inorganically filled, glass fiber reinforced, high dimensional stability at raised temperature, good media resistance, heat-resistant.Application areas: Thermally and dyna..