Polymer Property : Ball Indentation Hardness = 39.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Ball Indentation Hardness 39.0 MPa
5660 psi
dry; ISO 2039-1
EMS-Grivory Grivory® 2D 25 W 20 HL X black 9992 PA612-I
Product Description: Grilamid 2D 25 W 20 HL X black 9992 is a semi-flexible high viscosity, plasticized, high impact and highly heat resistant polyamide 612 (PA612) grade. Unique properties of Gril..
Ball Indentation Hardness 39.0 MPa
5660 psi
dry; ISO 2039-1
EMS-Grivory Grivory® 2D 25 W 20 X black PA612-I
Product Description: Grilamid 2D 25 W 20 X black 9992 is a semi-flexible high viscosity, plasticized, high impact, heat and UV resistant extrusion grade based on polyamide 612 (PA612). Unique proper..
Ball Indentation Hardness 39.0 MPa
5660 psi
dry; ISO 2039-1
EMS-Grivory Grivory® 2D 25 W 20 X nat PA612-I
Product Description: Grilamid 2D 25 W 20 X natural 9992 is a semi-flexible high viscosity, plasticized, high impact, heat and UV resistant extrusion grade based on polyamide 612 (PA612). Unique pro..
Ball Indentation Hardness 39.0 MPa
5660 psi
ISO 2039-1
Azoty Tarnow™ TARFLEN SM-S15G2 PTFE
Tarflen SM1 reinforced with 15% glass fibers and 2% graphite for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.