Polymer Property : Ball Indentation Hardness = 36.0 MPa
Polymer Property :
Ball Indentation Hardness =
36.0 MPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Ball Indentation Hardness
34.0
-
36.0
MPa
4930
-
5220
psi
ISO 2039-1
Adamas Hardor® 991 PE-UHMW
Information provided by Adamas, HPM