Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 227 MPa @Load 36.5 kg, Time 30.0 sec |
32900 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
BASF Ultrason® E 2010 C6 30% Carbon Filled Carbon fibers and Ultrason® two partners with good properties. The combination of carbon fibers with the amorphous high-temperature plastic Ultrason® guarantees mechanical properties for temperatu.. |