Polymer Property : Ball Indentation Hardness = 30300 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Ball Indentation Hardness 209 MPa
30300 psi
ISO 2039-1
Lanxess Durethan® BKV 30 G W1 901317 Nylon 6, Glass Fiber Reinforced
PA 6, 30% glass fibers, injection molding, weather stabilizedInformation provided by LANXESS.