Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 150 - 192 MPa | 21800 - 27800 psi | Average value: 171 MPa Grade Count:5 |
Overview of materials for Acetal Homopolymer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced". Each property range of values reported is minimum and maximum values .. |