Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 153 - 190 MPa | 22200 - 27600 psi | Average value: 179 MPa Grade Count:5 |
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled". Specific grades with glass content between 15.. |
|||
Ball Indentation Hardness | 153 MPa | 22200 psi | DIN 2039 |
Wolf Kunststoff ZEDEX® ZX-100MT A1T Polymer Alloy, Mineral Reinforced Stiff; Hard; Very high strength; No fiber reinforcementApplications: Handling, Vessel and Pump, Steel and Water, Chemical Engineering, Automotive Technology, Machine ToolsInformation provided by Zed.. |
|||
Ball Indentation Hardness | 153 MPa | 22200 psi | ISO 2039-1 |
BASF Ultradur S 4090 G4 20% Glass Filled PBT Ultradur S 4090 G4 is a 20% glass reinforced PBT+ASA blend. It produces moldings with good surface finish,is resistant to chemicals and stress cracking, and has low shrinkage and warpage.Applicatio.. |