Polymer Property : Ball Indentation Hardness = 21540 psi
Polymer Property :
Ball Indentation Hardness =
21540 psi
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Ball Indentation Hardness
148.5
MPa
21540
psi
GB3398
Beijing Evergrow Resources MoS2 Filled Nylon
Information provided by Beijing Evergrow Resources.