Polymer Property : Ball Indentation Hardness = 21025 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Ball Indentation Hardness 144.96 MPa
21025 psi
ISO 2039/1,2
Ensinger Tecaform™ SAN Polyacetal (POM)
TECAFORM™ (Polyacetal) and TECAPRO™ SAN (Polypropylene), provide an additional safety factor in reducing incidence of bacterial contamination. The raw materials are charged with an antimicrobial ..