Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 75.0 - 210 MPa | 10900 - 30500 psi | Average value: 141 MPa Grade Count:6 |
Overview of materials for Nylon 66/6, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are incl.. |
|||
Ball Indentation Hardness | 130 - 210 MPa | 18900 - 30500 psi | Average value: 158 MPa Grade Count:14 |
Overview of materials for Nylon 6, MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria.. |