Polymer Property : Ball Indentation Hardness = 206 MPa
Polymer Property :
Ball Indentation Hardness =
206 MPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Ball Indentation Hardness
206
MPa
29900
psi
dry; ISO 2039-1
EMS-Grivory Grivory® TSGZ-25/4 PA666-GF25
Information provided by EMS Grivory