Polymer Property : Ball Indentation Hardness = 192 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Ball Indentation Hardness 192 MPa
27800 psi
ISO 2039-1
BASF Ultrason® E 2010 MR HP PESU
Description: Unreinforced, medium viscosity standard injection molding grade for improved demolding behavior with Mold Release. PES-Blend with improved processibility. (High Productivity) Abbreviate..