Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 181 MPa | 26300 psi | ISO 2039-1 |
Nilit FRIANYL B63 CV40 Nylon 6.6 for injection molding, 40% carbon fiber reinforced Nylon 6.6 for injection molding, good conductive and electrostatic properties.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 181 MPa | 26300 psi | ISO 2039-1 |
BASF Ultramid® B35G3 BK 00564 15% Glass Filled PA6 (Conditioned) Description: 15% glass fiber reinforced injection molding grade e.g. for internal gas pressure applications such as flashing direction switch gears, automobile mirror housings and wheels of mountain.. |
|||
Ball Indentation Hardness | 181 MPa | 26300 psi | ISO 2039-1 |
BASF Ultramid® B35G3 BK 00564 15% Glass Filled PA6 (Dry) Description: 15% glass fiber reinforced injection molding grade e.g. for internal gas pressure applications such as flashing direction switch gears, automobile mirror housings and wheels of mountain.. |