Mechanical Properties Metric English Comments
Ball Indentation Hardness 173 MPa
25100 psi
ISO 2039-1
Nilit FRIANYL A63 FK 2010 Nylon 6.6 for injection molding, 20% glass fiber and 10% glass ball reinforced
Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics