Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 163 MPa | 23600 psi | ISO 2039-1 |
Nilit FRIANYL A63 AL40 Nylon 6.6 for injection molding, 40% aluminum filled Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 163 MPa | 23600 psi | ISO 2039-1 |
Nilit FRIANYL A63 TF-KV 1530 Nylon 6.6 for injection molding, 15% PTFE lubricated and 30% glass ball reinforced Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 163 MPa | 23600 psi | DIN 53456 |
Zell-Metall Engineering Plastics Zellamid 1100 Zellamid® 1100 is the registered trademark for Zell-Metalls cast nylon 6 in different qualities.Our standard quality is a heavy duty, high impact, wear and heat resistant polyamide. It offers .. |