Mechanical Properties Metric English Comments
Ball Indentation Hardness 162 MPa
23500 psi
ISO 2039-1
Nilit FRIANYL A63 H-SG40 Nylon 6.6 for injection molding, 40% mineral filled
Nylon 6.6 for injection molding, heat stabilized (dark natural color).Information provided by Frisetta Polymer, which merged into Nilit Plastics