Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 143 MPa | 20700 psi | 358 N; ISO 2039-1 |
Azoty Tarnow™ TARNOFORM 300 M POM Tribological modified grade with addition of molybdenum disulphide, which causes decreased coefficient of friction and wear, especially for applications requiring high load at low sliding speed.Info.. |