Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 123 MPa | 17800 psi | ISO 2039-1 |
Nilit FRIANYL A63 S Nylon 6.6 for injection molding Nylon 6.6 for injection molding, impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |