Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | 58.0 MPa @Temperature 23.0 °C |
8410 psi @Temperature 73.4 °F |
3% yield point; Orientation not specified; ASTM D882-91 |
DuPont™ Kapton® 250FN029 Polyimide/FEP Composite Film 250 Gauge film structure consisting of a 50 µm (2 mil) base polyimide film with a 13 µm (0.5 mil) coating of Teflon® FEP on one side.Kapton® Type HN film coated with Teflon® FEP fluoropolymer r.. |