Polymer Property : Charpy Impact = 94.9 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact 94.9 J

@Tempering Temp. 704 °C
70.0 ft-lb

@Tempering Temp. 1300 °F
oil quenched from 1525°F then tempered
Crucible Steel Holder Block Steel, AISI 4150 Modified
Crucible Holder Block is a prehardened (26/30 HRC) free machining medium alloy steel intended for holders or backers for plastic molds, die casting dies, and cold or hot forming tools. It may also b..