Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | >= 88.1 J @Temperature 20.0 °C |
>= 65.0 ft-lb @Temperature 68.0 °F |
|
Schmolz + Bickenbach LeanDupâ„¢ 35N Stainless Steel Bar Description: LeanDupâ„¢ 35N also known as (Uranus 35 N) is a dual phase austentic-ferritic stainless steel that has the ability to become as important as 316L. It offers better corrosion resistan.. |