Charpy Impact 118 J

@Treatment Temp. 427 °C,
Time 1.44e+7 sec
87.0 ft-lb

@Treatment Temp. 801 °F,
Time 4000 hour
Room temp test after thermal exposure
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate, Age-hardened
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..