Mechanical Properties Metric English Comments
Charpy Impact 56.9 J

@Tempering Temp. 427 °C
42.0 ft-lb

@Tempering Temp. 800 °F
hardened at 1475°F then tempered; C-notch
Crucible Steel HALGRAPH® Tool Steel, AISI O6
Halgraph is an oil-hardening graphitic tool steel with excellent non-deforming properties. Free graphite in its structure affords exceptional free-machining properties. The combination of graphite a..