Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 66.4 J @Tempering Temp. 149 °C |
49.0 ft-lb @Tempering Temp. 300 °F |
hardened at 1650°F then tempered; C-notch |
Crucible Steel LABELLE® Silicon #2 Tool Steel LaBelle Silicon #2 is a shock resisting tool steel capable of maximum toughness at relatively high hardness. It has excellent resistance to impact and battering, with good edge retention.Information.. |