Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 54.2 J @Treatment Temp. 551.7 °C |
40.0 ft-lb @Treatment Temp. 1025 °F |
hardened H1025; V-notch |
Crucible Steel 174 SXR Precipitation Hardening Stainless Steel Crucible 174 SXR is a premium quality precipitation- hardening stainless steel designed for use as rifle barrels. It is a modification of Crucible’s 17Cr-4Ni which offers substantially improved mac.. |