Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact = 260 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact >= 353 J

@Temperature 25.0 °C
>= 260 ft-lb

@Temperature 77.0 °F
No thermal exposure
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate, Annealed
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Charpy Impact >= 353 J

@Treatment Temp. 427 °C,
Time 3.60e+6 sec
>= 260 ft-lb

@Treatment Temp. 801 °F,
Time 1000 hour
Room temp test after thermal exposure
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate, Annealed
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Charpy Impact >= 353 J

@Treatment Temp. 427 °C,
Time 2.88e+7 sec
>= 260 ft-lb

@Treatment Temp. 801 °F,
Time 8000 hour
Room temp test after thermal exposure
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate, Annealed
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..