Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 24.4 J @Tempering Temp. 566 °C |
18.0 ft-lb @Tempering Temp. 1050 °F |
air cooled from 1850°F then tempered; V-notch |
Crucible Steel HALCOMB® 218 Tool Steel, AISI H11 Halcomb 218 is a general purpose hot work tool steel, combining good toughness with moderate high-temperature strength and heat check resistance. Because of its high toughness, it is particularly su.. |