Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact = 20.3 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact >= 20.3 J

@Treatment Temp. 551.7 °C,
Time 14400 sec
>= 15.0 ft-lb

@Treatment Temp. 1025 °F,
Time 4.00 hour
Schmolz + Bickenbach UGIMA® 630 Stainless Steel Bar
Description: 630 UGIMA® is an improved machining martensitic precipitation hardenable grade produced only by Ugitech. It is identical in every way to standard type 630 (17-4), except with respect..
Charpy Impact 20.3 J

@Temperature 538 °C
15.0 ft-lb

@Temperature 1000 °F
48-50 HRC; V-notch
Crucible Steel HALCOMB® 425 Tool Steel, AISI H19
Halcomb 425 is designed for higher operating temperatures than H13, where wear resistance and heat check resistance are more critical than toughness. While H19 has excellent heat checking resistance..
Copyright © lookpolymers.com All Rights Reserved