Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 212 J @Tempering Temp. 371 °C |
156 ft-lb @Tempering Temp. 700 °F |
hardened at 1650°F then tempered; C-notch |
Crucible Steel LABELLE® Silicon #2 Tool Steel LaBelle Silicon #2 is a shock resisting tool steel capable of maximum toughness at relatively high hardness. It has excellent resistance to impact and battering, with good edge retention.Information.. |