Charpy Impact 151 J

@Temperature 25.0 °C
111 ft-lb

@Temperature 77.0 °F
No thermal exposure
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate, Age-hardened
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..